Density (g/cm3) |
5.08 |
Melting Point (K) |
1116 |
Thermal Expansion Coefficient (10-6/°C) |
8 along C-axis |
Cleavage Plane |
<100> |
Hygroscopic |
Yes |
Wavelength of Emission Max. (nm) |
380 |
Refractive Index @ Emission Max |
~1.9 |
Primary Decay Time (μs) |
0.016 |
Light Yield (Photons/keVγ) |
63 |
Photoelectron Yield (% of NaI(Tl)) (for γ-rays) |
165 |